Mike Durling wrote:
>
> My M4 also shows definate glue residue under the cracked-off pieces of
> vulcanite. Perhaps the LTM models had their vulcanite put on differently
> and that's why they are less prone to crack. (at least that's my
> experience)
>
> Mike D
>
It has been my understanding that the vulcanite was glued on the cameras but
that the material was warmed up to make it plyable otherwise it would crack
when being applied. I do know that under heat it does get soft and you can
bend it without cracking it.
John Shick
Replies:
Reply from Javier Perez <summarex@yahoo.com> (Re: Vs: Vulcanite: [Leica] Friday FS: Nickel + Dime)
In reply to:
Message from "Raimo Korhonen" <raimo.korhonen@pp2.inet.fi> (Vs: Vulcanite: [Leica] Friday FS: Nickel + Dime)
Message from Javier Perez <summarex@yahoo.com> (Re: Vs: Vulcanite: [Leica] Friday FS: Nickel + Dime)
Message from "Mike Durling" <durling@widomaker.com> (Re: Vs: Vulcanite: [Leica] Friday FS: Nickel + Dime)